Tempered glass: why a phone does not break a car window
A cell phone did not break the window in MythBusters' "Underwater Car" test. The episode premiered on January 24, 2007, and the MythResults episode guide lists the phone among several objects tried against a car's tempered side window, with the result recorded as ineffective. Keys and steel-toed boots were tried too, and both also failed. The guide explains the pattern in one phrase: tempered glass resists blunt impact.
That episode covered a longer list of beliefs about escaping a sunken car. The first was that a submerged car's door cannot be opened until the interior has flooded. MythResults marks it confirmed: the pressure difference is too great for a man to force the door, so the interior must flood first. In the first test, Adam needed emergency air. In a second test, he escaped by opening the door, but only by staying calm and waiting until the cabin was well flooded to conserve oxygen.
The window tests followed the same logic. A manual crank window was busted. A 350 pound test weight, equal to the pressure difference at two feet of immersion, pressed the glass against the frame so hard that no effort could move the gear, and the handle was more likely to break. Power windows were more powerful but still could not overcome the pressure difference, although they withstood prolonged fresh-water immersion and still worked.
Breaking the glass was the remaining route. Keys, a cell phone and steel-toed boots were all busted as methods. Two purpose-built tools were confirmed. A window-breaking hammer, whose pointed tip is designed to shatter tempered glass, broke the window on the first try. A spring-loaded center punch, which works on the same principle and is sold for the purpose, also broke it on the first try.
Why tempered glass behaves this way is a manufacturing story. McGill University's Office for Science and Society describes two kinds of safety glass, laminated and tempered. Tempered glass is heated and then quickly quenched, which makes it strong and shatter-resistant. Scientific American adds the detail: after the glass has been cut to its final size, it goes into a tempering oven and is heated to over 600 degrees Celsius, with 620 as the industry standard. Within seconds, high-pressure air blasts both surfaces.
The quench cools the outer surfaces much faster than the center. As the center cools, it pulls back from the outer surfaces, which leaves the center in tension and the outer surfaces in compression. Glass in tension breaks about five times more easily than glass in compression, so the compressed skin is what protects the pane. Scientific American puts tempered glass at about four times stronger than annealed glass. Annealed glass breaks at 6,000 psi, while federal specifications require tempered glass to have a surface compression of at least 10,000 psi, and it generally breaks at about 24,000 psi.
When tempered glass does fail, it fails completely. Unlike annealed glass, which breaks into jagged shards, tempered glass fractures into small, relatively harmless pieces. Manufacturers even test by punching a sample and checking that it breaks into many small, similarly sized pieces, because the break pattern shows whether the tempering was done properly. Cutting or edging tempered glass after heat treatment can reduce its strength or cause it to fail, which is why the glass is cut to size first.
Chemical tempering is an alternative. It exchanges ions on the glass surface to create compression, and Scientific American says it is not widely used because it costs far more than oven-and-quench tempering. McGill describes the same alternative: a bath of molten potassium nitrate exchanges sodium ions in the glass for potassium ions, producing a very tough glass. McGill traces the original idea to a mid-19th-century experiment by Francois Barthelemy Alfred Royer de la Bastie, in which no accident was involved. The original method was to heat glass until it melted and then cool it quickly.
Laminated glass has a different history and a different job. In 1903, French chemist Edouard Benedictus dropped a glass flask. It shattered, but the fragments did not fly apart. The flask had held an alcohol solution of collodion, and when the solvent evaporated, a plastic film remained inside. Benedictus later spent a night making a glass coating after reading about a young girl cut by glass in an early automobile accident. Within a day he had produced the first sheet of safety glass, which he named triplex, with a cellulose nitrate film between two glass sheets. He applied for a patent in 1909.
Triplex's first practical use was in the face shields of World War I gas masks, and by the 1920s it was standard in American automobiles. In 1933 cellulose acetate replaced cellulose nitrate, which had yellowed with age; McGill says the acetate was not quite as strong but did not yellow. Poly(vinylbutyral), a synthetic resin, was later found to be superior and has been the standard windshield material since 1939.
That is why a car carries both kinds of glass. McGill states that car windshields are generally laminated and side windows are generally tempered. Scientific American lists side and rear vehicle windows among the main uses of tempered glass, alongside entrance doors, shower enclosures, racquetball courts and microwave ovens. The side window the MythBusters team tested was made of the material that is built to resist exactly the kind of blunt tap a phone can deliver.
- MythResults, MythBusters Episode 72: Underwater Car — mythresults.com
- McGill University Office for Science and Society, What is Safety Glass? — www.mcgill.ca
- Scientific American, How is tempered glass made? — www.scientificamerican.com